Item |
Description |
|
Symptom |
Tramp iron captured by the self-cleaning magnet lands in the product chute, tail chute, or floor instead of the iron discharge chute |
|
Typical Trigger |
Conveyor belt replacement, belt speed change, pulley lagging renewal, or structural realignment |
|
Root Cause Category |
Geometry drift: gap, release point, trajectory, chute position |
|
First Checks |
New belt thickness, magnet gap, chute lip position, cleat condition, belt speed |
|
Time to Diagnose |
Usually 2–4 hours with a landing grid test |
|
Typical Fix |
Re-shim magnet height, re-align chute lip/splitter plate, re-run commissioning test |
|
Risk if Ignored |
Product contamination, downstream crusher damage, chute plugging, lost production |
|
Related Equipment |
Self-Cleaning Electromagnetic Separator, Electromagnetic Overband Separator, Iron Magnet |
The discharge problem in this article is a maintenance problem, and this week's industry news shows why maintenance discipline matters more as margins tighten:
· LME copper fell 3.7% on November 18 to about $12,742/t, the lowest since early May, and LME tin dropped 7.33% to $41,755/t — a broad metals pullback that pressures processor margins.
· Spot gold fell 2% intraday to about $3,772/oz, its lowest since late September 2025, while silver traded near $46/oz, down roughly 12% over the week.
· Iron ore spot in the domestic market held near ¥644/t day-on-day but remains about 20% lower year over year, keeping cost-per-tonne discipline at the front of every plant manager's agenda.
· Capstone Copper reported that major mechanical repairs to the primary crusher at its Pinto Valley mine pushed the restart to mid-December, with mobile crushing bridging the gap — a reminder that one major wear component can idle an entire operation.
· FLSmidth signed an agreement to acquire crushing equipment manufacturer CE Africa (announced November 16), continuing the industry shift toward aftermarket service and wear-part lifecycle value.
· A major steel group's mining division broke ground on a 4.5 km, 7.2 Mt/a belt conveying system to replace rail haulage — confirming that conveyor infrastructure and its protection equipment remain active investment areas.
Sources note: figures compiled from public market reporting on November 18–19, 2026; verify live prices before making procurement decisions.
Direct answer: a self-cleaning magnet discharges iron where the belt surface carries it, and a belt replacement moves the belt surface. Everything downstream of that one change follows automatically.
An overband separator does not decide where iron goes with electronics or sensors. The self-cleaning belt's cleats grip each captured piece and carry it around the magnet block. The piece stays attached until the magnetic field weakens past the edge of the magnetic zone — at the discharge roller on the non-magnetic side. From that release point, the piece leaves on a ballistic trajectory set by its tangential velocity and the pulley geometry, and the chute lip must sit exactly under that trajectory. Five geometry variables change when you replace a belt:
|
Geometry Variable |
Old Worn Belt |
New Belt |
Effect on Iron Discharge |
|
Belt top height above stringer |
Lower (cover worn 3–8 mm) |
Higher by full cover + carcass difference |
Gap shrinks; iron release point shifts forward |
|
Belt stiffness / tension |
Stretched, lower tension |
Stiffer, higher tension |
Take-up moves; pulley wrap changes slightly |
|
Belt sag between idlers |
More sag |
Less sag |
Belt line flatter; capture zone edge moves |
|
Surface friction |
Glazed, polished |
Fresh rubber, higher friction |
Iron rides further before release |
|
Weight of iron against belt |
—— |
—— |
Thicker belt resists attraction; lighter steel may not reach belt surface |
The second-order effect is the one that surprises crews: because the fresh belt surface is higher and more grippy, captured iron travels 20–60 mm further around the discharge roller before separating. If the chute lip was set for the old release point, iron now arcs over the chute opening and lands behind it — typically into the product chute or onto the walkway. Nothing is "broken"; the machine is simply obeying the new geometry. This is why any plant running a self-cleaning overband electromagnetic unit should treat belt replacement and magnet re-commissioning as one job, not two.
![]()
Customer Type: Iron ore processing plant, 1,600 mm trunk conveyor feeding secondary crushing
Ore Type: Magnetite iron ore, high tramp iron incidence from mining front
Operating Conditions: 1.8 m/s belt speed, 2,000 t/h, bed depth ~180 mm, cross-belt electromagnetic separator over the head section
Problem: After the annual belt replacement (fabric belt upgraded from 4-ply to 5-ply), captured tramp iron began arcing over the reject chute lip and landing in the product transfer chute. Within two days, operators recovered steel fragments from the SAG mill feed belt; one near-miss with a pump impeller forced a 6-hour unplanned stoppage.
Solution: A landing grid test showed the release point had rotated forward by approximately 45 mm due to the thicker belt closing the magnet gap from 320 mm to 288 mm and the fresh high-friction cover holding iron longer around the discharge roller. The crew re-shimmed the magnet frame to restore a 300 mm gap, moved the chute lip 60 mm forward on new slotted brackets, and reset the splitter plate that had been re-hung 30 mm off position during the belt work.
Result: Follow-up grid test captured 96% of test pieces in the reject chute (from 61% before correction); zero steel recovered from downstream equipment over the following 90 days; total correction time 3.5 hours, of which 2 hours were production-free. The plant now runs the landing grid test at every belt change as standard practice.
Q1: Why did the magnet only start mis-discharging after the belt was replaced?
A: The magnet's release point is geometry-dependent. The new belt's thickness, stiffness and surface friction moved the release point 20–60 mm, which was enough to carry iron past the chute lip. The magnet itself never changed; the conveyor geometry did.
Q2: How much can a new belt realistically shift the iron landing point?
A: Field experience shows 20–60 mm from thickness and friction changes alone, and 100 mm or more if belt speed also changed. A landing grid test measures the actual shift in your plant rather than estimating it.
Q3: Can I just move the chute instead of adjusting the magnet?
A: Yes, if the capture rate is still acceptable. Moving the chute lip under the new trajectory is often faster. But if the gap changed by more than 20 mm, correct the gap too — capture performance and trajectory are linked through the same geometry.
Q4: What if iron lands in two places instead of one?
A: Scattered landings usually mean mixed piece behavior: heavy lumps hold to the discharge roller and fly far, light slivers release early and drop short. Two capture points — overband plus a magnetic pulley — solve this better than chasing a single chute position.
Contact: Annie Lu
Email: annie.lu@huataogroup.com
Phone / WhatsApp: +86 180 3242 2676
Website: http://www.tufflexscreen.com
We warmly welcome customers from around the world to contact us and establish mutually beneficial partnerships.
Contact Person: Mr. Maple
Tel: +86 17778255675
Fax: 86--311-80690567